Mechanical Properties Metric English Comments
Modulus of Elasticity 173 GPa

@Temperature 700 °C
25100 ksi

@Temperature 1290 °F
Dynamic
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Modulus of Elasticity 173 GPa

@Temperature 600 °C
25100 ksi

@Temperature 1110 °F
Dynamic
Haynes 617 Nickel Alloy Plate
Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed..