Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 151.8 GPa @Temperature 550 °C |
22020 ksi @Temperature 1020 °F |
|
Special Metals INCOLOY® Alloy 903 A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a.. |