Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 103.4 GPa @Temperature 23.0 °C |
15000 ksi @Temperature 73.4 °F |
|
ATI Wah Chang TI-3Al-2.5V Ti-3Al-2.5V has proved to be a sufficiently malleable material for tube manufacture. It can be cold worked by standard tube making processes, is weldable and can be strength-ended by cold working an.. |