Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 148.9 GPa @Temperature -195 °C |
21600 ksi @Temperature -319 °F |
|
Special Metals INCOLOY® Alloy 903 A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a.. |