Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 96.53 GPa @Temperature 788 °C |
14000 ksi @Temperature 1450 °F |
|
ATI Wah Chang TI-3Al-2.5V Ti-3Al-2.5V has proved to be a sufficiently malleable material for tube manufacture. It can be cold worked by standard tube making processes, is weldable and can be strength-ended by cold working an.. |