Mechanical Properties Metric English Comments
Modulus of Elasticity 12.4 GPa

@Thickness 1.57 mm
1800 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP193E Synthetic Fabric
Description: 17 oz. aramid and "soft glass" fibers are combined to make a fabric that is stronger than pure aramid and less abrasive than glass fabrics. This material is impregnated with a high temp..
Modulus of Elasticity 12.4 GPa

@Thickness 1.57 mm
1800 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP329 Cotton Fabric
Description: Bleached linen with melamine resin system. Provides better arc resistance than NP320E. Also, resistant to ammonia based refrigerants. Hard, durable material should be heated to punch, ..
Modulus of Elasticity 12.4 GPa

@Thickness 1.57 mm
1800 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP504 Glass Fabric
Description: Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. Capable of continuous operation at 175° C, see note..
Modulus of Elasticity 12.4 GPa

@Thickness 1.57 mm
1800 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP634 Laminate
Description: Warm punching, composite grade with woven glass covers for improved flexural, tensile and impact strength. Electrical properties comparable to NP611.Thickness Tested: 0.062", 0.125" and..