Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 75.2 GPa @Temperature 260 °C |
10900 ksi @Temperature 500 °F |
|
ATI Wah Chang Zircadyne® Alloy Zr 702 Zircadyne 702 is commercially pure zirconium. Alloy exhibits good ductility even at cryogenic temperatures and good strength comparable with other common engineering alloys.Information provided by A.. |