Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.01 J/cm @Temperature -30.0 °C |
9.39 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® IP300 PC Improved toughness/impact strength at ambient/low temperatures for automotive instrument panels, knee bolsters and trim. Range gray and black only.This data was supplied by SABIC-IP for the America.. |