Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.08 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® AD4820 PC LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin.This data was supplied by SABIC-IP for the America.. |
|||
Izod Impact, Notched | 9.08 J/cm @Temperature 22.8 °C |
17.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-IM1 Polycarbonate, Impact Modified, Low Flow Polycarbonate, Impact Modified, Low FlowProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Izod Impact, Notched | 9.08 J/cm @Temperature 22.8 °C |
17.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-IM1-UV Polycarbonate, Impact Modified, Low Flow, UV-stabilized Polycarbonate, Impact Modified, Low Flow, UV-stabilizedProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Izod Impact, Notched | 9.08 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXD103 PC FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Notched | 9.08 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXD103 PC (Asia Pacific) FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Notched | 9.08 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXD103 PC (Europe-Africa-Middle East) FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Notched | 9.08 J/cm @Temperature 22.8 °C |
17.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol 6608-LLT Nylon 66, High Impact Modified, Lubricated, Low Temp Impact Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 9.08 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
17.0 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 9246 Rigid PVC, Molding Georgia Gulf 9246 is a high impact compound suitable for food packaging.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 9.08 J/cm @Thickness 6.35 mm |
17.0 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 5055 Rigid PVC, Extrusion, White Georgia Gulf 5055 White is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical ResistantOutdoor.. |
|||
Izod Impact, Notched | 9.08 J/cm @Thickness 6.35 mm |
17.0 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 7555 Rigid PVC, Extrusion, Natural Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn.. |
|||
Izod Impact, Notched | 9.08 J/cm @Thickness 6.35 mm |
17.0 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 7555 Rigid PVC, Extrusion, White Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn.. |
|||
Izod Impact, Notched | 9.08 J/cm @Thickness 6.35 mm |
17.0 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 5055 Rigid PVC, Extrusion, Natural Georgia Gulf 5055 is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical RetardantInformation p.. |