Mechanical Properties Metric English Comments
Izod Impact, Notched 4.75 J/cm

@Temperature 0.000 °C
8.90 ft-lb/in

@Temperature 32.0 °F
ASTM D 256
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Asia Pacific)
XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Asia Pacific reg..
Izod Impact, Notched 4.75 J/cm

@Temperature 0.000 °C
8.90 ft-lb/in

@Temperature 32.0 °F
ASTM D 256
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East)
XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi..
Izod Impact, Notched 4.75 J/cm

@Temperature 23.0 °C
8.90 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 360E0096914 Cellulose Acetate Propionate, Natural, Trsp
Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
Izod Impact, Notched 4.75 J/cm

@Temperature 23.0 °C
8.90 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 360E4861314 Cellulose Acetate Propionate, Clear, Trsp
Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..