Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.59 J/cm @Temperature -20.0 °C |
16.1 ft-lb/in @Temperature -4.00 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EXRL0683 PC Copolymer 11 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |