Mechanical Properties Metric English Comments
Izod Impact, Notched 8.17 J/cm

@Temperature 23.0 °C
15.3 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was suppli..