Mechanical Properties Metric English Comments
Izod Impact, Notched 4.31 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
8.08 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical SH625 ABS, High Impact, High Flow
Feature: Extrusion Molding, High Impact, High FlowApplication: Ski Flat, MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 4.31 J/cm

@Thickness 3.17 mm
8.08 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® SD-0170 F ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 4.31 J/cm

@Thickness 3.17 mm
8.08 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® SV-0167 ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 4.31 J/cm

@Thickness 3.17 mm
8.08 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® SD-0170 F ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 4.31 J/cm

@Thickness 3.17 mm
8.08 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® SV-0167 ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.