Polymer Property : Izod Impact, Notched = 7.31 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 7.31 J/cm

@Temperature 23.0 °C
13.7 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Ovation Polymers Nima™ NH PC143P Polycarbonate
Non-Hal FR-PC with High impact and improved processabilityAll properties after 48hrs conditioning at 23°C/50% RH