Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.20 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
13.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87350 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 7.20 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
13.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87850 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 7.20 J/cm @Temperature -30.0 °C |
13.5 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® ML7647 PC Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 7.20 J/cm @Temperature -30.0 °C |
13.5 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® ML7647 PC (Europe-Africa-Middle East) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 7.20 J/cm @Temperature 0.000 °C |
13.5 ft-lb/in @Temperature 32.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East) XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab.. |
|||
Izod Impact, Notched | 7.20 J/cm @Temperature -29.0 °C |
13.5 ft-lb/in @Temperature -20.2 °F |
3.2 mm (0.125 in) notch |
Kraton® G1652 + PPE blend (20/80) Blending KRATON D and G polymers with PPE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [.. |
|||
Izod Impact, Notched | 7.20 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
13.5 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
transverse direction; ISO 180 |
Azdel Plus U421-B01 42% Directionalized Continuous Fiber Mat / PP Resin Matrix AZDEL® U421-B01 is a glass mat thermoplastic laminate based upon a combination of random oriented continuous fiber mat and oriented fiber mat contained within a polypropylene resin matrix. This co.. |
|||
Izod Impact, Notched | 7.20 J/cm @Temperature -30.0 °C |
13.5 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EXL1033C PC Copolymer Lexan*EXL1033C polycarbonate (PC) siloxane copolymer resin is a low flow, UV stabilized grade designed for (co)-extrusion. This resin offers low temperature (-30C) ductility and excellent extrusion .. |