Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.99 J/cm @Temperature 0.000 °C |
13.1 ft-lb/in @Temperature 32.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® EXRL0672 PC Copolymer 40 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |