Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.75 J/cm @Temperature 23.0 °C |
12.6 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East) XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab.. |