Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 6.50 J/cm

@Temperature 23.0 °C
12.2 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS
Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 6.50 J/cm

@Temperature 23.0 °C
12.2 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Asia Pacific)
Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 6.50 J/cm

@Temperature 23.0 °C
12.2 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Europe-Africa-Middle East)
Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 6.50 J/cm

@Temperature -30.0 °C
12.2 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® ML7652 PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. Medium flow, excellent low temperature ductility.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 6.50 J/cm

@Temperature 23.0 °C
12.2 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)  (Unverified Data**)
Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper..
Izod Impact, Notched 6.50 J/cm

@Temperature 23.0 °C
12.2 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC
Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im..
Izod Impact, Notched 6.50 J/cm

@Temperature 23.0 °C
12.2 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tritan EX401 Copolyester
Eastman Tritan EX401 is an amorphous copolyester with excellent appearance and clarity. Tritan EX401 contains a mold release derived from vegetable based sources. Its most outstanding features are..
Izod Impact, Notched 6.50 J/cm

@Temperature 23.0 °C
12.2 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tritan LX201 Copolyester
Eastman Tritan LX201 is an amorphous copolyester with excellent appearance and clarity. Tritan LX201 contains a mold release derived from vegetable based sources. Its most outstanding features are..