Polymer Property : Izod Impact, Notched = 6.22 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 3.32 J/cm

@Thickness 3.17 mm
6.22 ft-lb/in

@Thickness 0.125 in
ASTM D256
Chi Mei Polylac® PA-746 ABS - High Flow
High flow, medium impact
Izod Impact, Notched 3.32 J/cm

@Thickness 3.17 mm
6.22 ft-lb/in

@Thickness 0.125 in
ASTM D256
Chi Mei Polylac® PA-747F ABS - Extrusion
Refrigerator