Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.30 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
6.18 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87358 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |