Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.26 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
6.10 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Styron INSPIRE™ TF3800 Polypropylene Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |