Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.19 J/cm @Temperature 23.0 °C |
5.98 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® 357 PBT PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.This data was supplied by SABIC-IP for the Americas region. |