Mechanical Properties Metric English Comments
Izod Impact, Notched 3.14 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
5.88 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical HF380I ABS, High Flow
Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 3.14 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
5.88 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical MU620 ABS, Low Deformation
Feature: Extrusion Molding, Low DeformationApplication: Mock-UpCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 3.14 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
5.88 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical MA221 ABS, High Impact, Low Gloss
Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 3.14 J/cm

@Temperature 0.000 °C
5.88 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SCG Chemicals EL-Leneâ„¢ H1000PC High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stability, low sagging, good balance of MRS, SCG, and RCPRecommended Applications: Water pressure and gas pipesCertification: Certified by EXOVA..