Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.51 J/cm @Temperature 23.0 °C |
4.70 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 2.51 J/cm @Temperature 23.0 °C |
4.70 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 2.51 J/cm @Temperature 23.0 °C |
4.70 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Europe-Africa-Middle East) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |