Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.05 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
7.59 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PP 1370 PRE-ELEC PP 1370 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |