Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.95 J/cm @Temperature -29.0 °C |
7.40 ft-lb/in @Temperature -20.2 °F |
3.2 mm (0.125 in) notch |
Kraton® G1651 + PPE blend (20/80) Blending KRATON D and G polymers with PPE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [.. |