Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.79 J/cm @Temperature 23.0 °C |
7.10 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl MX5569 PPE+PS PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-.. |