Mechanical Properties Metric English Comments
Izod Impact, Notched 3.3333 J/cm

@Thickness 3.20 mm
6.2446 ft-lb/in

@Thickness 0.126 in
ASTM D-256
Bhansali Engineering Abstron IM-11G ABS Injection Molding Grade
High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali
Izod Impact, Notched 3.3333 J/cm

@Thickness 3.20 mm
6.2446 ft-lb/in

@Thickness 0.126 in
ASTM D-256
Bhansali Engineering Abstron IM-11G ABS Injection Molding Grade
High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali