Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 12.4 J/cm @Thickness 3.17 mm |
23.3 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 7768 Rigid PVC, Extrusion Georgia Gulf 7768 is a general purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityDimen.. |