Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.3725 J/cm @Thickness 6.40 mm |
2.5713 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron KU-650M ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.3725 J/cm @Thickness 6.40 mm |
2.5713 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron KU-650 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.3725 J/cm @Thickness 6.40 mm |
2.5713 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron KU-650M ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.3725 J/cm @Thickness 6.40 mm |
2.5713 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron KU-650 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |