Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.41 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.51 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa HR-527 Modified ABS Features:UL94 HB @ 1.5-3.2mmImpact resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |