Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.12 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.97 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa HF-626 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowHigh impact resistanceApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Izod Impact, Notched | 2.12 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.97 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa HR-527 Modified ABS Features:UL94 HB @ 1.5-3.2mmImpact resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |