Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87570 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 8.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M4300 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 8.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M4885 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 8.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding MR200 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 8.50 J/cm @Temperature 23.0 °C |
15.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® IFX2420Z PC (Asia Pacific) Lexan* IFX2420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware applications specifically for welding. This grades .. |
|||
Izod Impact, Notched | 8.50 J/cm @Temperature 23.0 °C |
15.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® IFX6420Z PC (Asia Pacific) Lexan* IFX6420Z is a medium viscosity, release containing, injection moldable, polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grades meets the transm.. |
|||
Izod Impact, Notched | 8.48 J/cm @Temperature 23.0 °C |
15.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer (Europe-Africa-Middle East) Transparent weatherable PC copolymer for blowmolding/extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 8.49 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
15.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
notch |
Kraton® G1651 + PC blend (5/95) Blending KRATON D and G polymers with PC significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |