Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.00 - 8.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.2 - 15.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon PC IX3000 Polycarbonate, High Impact Characteristics: high fluidity, high impact |
|||
Izod Impact, Notched | 6.00 - 8.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.2 - 15.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon PC UVR Polycarbonate, High Impact Characteristics: high fluidity, high impact, UV resistant |