Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 14.95 J/cm @Thickness 3.20 mm |
28.01 ft-lb/in @Thickness 0.126 in |
reverse notched; ASTM D 256 |
SABIC Innovative Plastics Ultem 1010KM PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 14.95 J/cm @Thickness 3.20 mm |
28.01 ft-lb/in @Thickness 0.126 in |
reverse notched; ASTM D 256 |
SABIC Innovative Plastics Ultem 1010KM PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 14.95 J/cm @Thickness 3.20 mm |
28.01 ft-lb/in @Thickness 0.126 in |
reverse notched; ASTM D 256 |
SABIC Innovative Plastics Ultem 1010KM PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |