Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 11.48 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
21.51 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
notch |
Kraton® G1657 + PA-6 blend (8/12/80) Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |