Polymer Property : Izod Impact, Notched = 10.06 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 10.06 J/cm

@Temperature 0.000 °C
18.85 ft-lb/in

@Temperature 32.0 °F
ASTM D256
Eastman Tritan GX100 Copolyester
Eastman Tritan copolyester GX100's strength, clarity and temperature resistance make it ideal for demanding applications. Extruded Sheet is manufactured with Eastman's Tritan copolyester GX100 resi..