Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.06 J/cm @Temperature -30.0 °C |
1.99 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® C1950 PC+ABS Low viscosity injection molding resin.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.06 J/cm @Temperature 23.0 °C |
1.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXM173R PC UV stabilized PC in special effects colors. Metallic and pearlescent additives. Color may affect performance.This data was supplied by SABIC-IP for the Americas region. |