Polymer Property : Izod Impact, Notched = 1.68 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.897 J/cm

@Temperature -20.0 °C
1.68 ft-lb/in

@Temperature -4.00 °F
1/8'' notched bar; ASTM D256
Ineos N02J-00 Polypropylene Impact Copolymer
This is a low melt flow rate, high impact copolymer polypropylene for sheet extrusion and thick wall injection molding applications. It offers a superior balance of stiffness and impact strength fo..