Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.810 J/cm @Temperature -30.0 °C |
1.52 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Asia Pacific) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the A.. |
|||
Izod Impact, Notched | 0.810 J/cm @Temperature -30.0 °C |
1.52 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the E.. |