Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.770 J/cm @Temperature -40.0 °C |
1.44 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar DN010 Copolyester Eastar Copolyester DN010 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN010 contains no mold release.Applications.. |
|||
Izod Impact, Notched | 0.770 J/cm @Temperature -40.0 °C |
1.44 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar DN011 Copolyester Eastar Copolyester DN011 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN011 contains a mold release.Applications/.. |