Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.747 J/cm @Temperature -40.0 °C |
1.40 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PPX-FRG30 Modified-PPO, V-1 Flame Retardant, 30% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 30% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Izod Impact, Notched | 0.747 J/cm @Temperature -17.8 °C |
1.40 ft-lb/in @Temperature 0.000 °F |
1/2" x 1/8"; ASTM-D256 |
Ineos ABS Lustran® Guardian™ 732 ABS, Extrusion Grade Lustran® Guardian™ ABS 732 is an extrusion grade resin designed for use in thermoformed refrigerator and freezer liner applications. It is suitable for use with 245fa PU foams. |
|||
Izod Impact, Notched | 0.747 J/cm @Thickness 6.35 mm, Temperature -40.0 °C |
1.40 ft-lb/in @Thickness 0.250 in, Temperature -40.0 °F |
ASTM-D256 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Izod Impact, Notched | 0.747 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.40 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF43 IM L BKN 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth.. |
|||
Izod Impact, Notched | 0.747 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.40 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES HiFill® PA4/6 HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.747 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.40 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES HiFill® PA4/6 HS LBK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackTPCI# 9651150Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.747 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.40 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Luriblend® PA4/6 HS L BK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedUL File Number: E157318Appearance: BlackInformation provided by TP Composites.. |
|||
Izod Impact, Notched | 0.747 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.40 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8011 Availability: North AmericaForms: PelletsFeatures: PlatableInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.745 J/cm @Temperature -20.0 °C |
1.40 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H5211PC High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good balance of MRS, SCG, and RCPRecommended Applications: Water pressure and gas pipesCertification: Certified by EXOVA, LNE, AENOR,.. |
|||
Izod Impact, Notched | 0.747 J/cm @Temperature -20.0 °C |
1.40 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Dow C702-20NA Polypropylene Impact Copolymer Resin OverviewHigh impact performanceContains a nucleating additiveContains an antistatic additiveComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C702-20NA Polypropylene Resin is intended f.. |
|||
Izod Impact, Notched | 0.747 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.40 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall SP-6340 Rigid PVC, Molding Georgia Gulf SP-6340 is a rigid vinyl injection molding compound designed for fittings and parts of similar confiation where maximum burst strength is required. Georgia Gulf 6340 is ideally suited .. |