Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 1.38 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.735 J/cm

@Thickness 3.17 mm
1.38 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® VB-5300GS PBT, Glass Filled FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.735 J/cm

@Thickness 3.17 mm
1.38 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® GR-4020 ABS, 20% Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.735 J/cm

@Thickness 3.17 mm
1.38 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® GR-4020 ABS, 20% Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.735 J/cm

@Thickness 3.17 mm
1.38 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® VB-5300GS PBT, Glass Filled FR
Information provided by Samsung Cheil Industries.
Copyright © lookpolymers.com All Rights Reserved