Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.500 - 0.600 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.937 - 1.12 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene |