Polymer Property : Izod Impact, Notched = 0.731 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.390 J/cm

@Temperature -40.0 °C
0.731 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Drystar 0827 Copolyester
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Izod Impact, Notched 0.390 J/cm

@Temperature -30.0 °C
0.731 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Eastman Spectar® 14471 Copolyester
Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use ..
Izod Impact, Notched 0.390 J/cm

@Temperature -20.0 °C
0.731 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
Braskem CP 404XP HECO Polypropylene Heterophasic Copolymer
CP 404XP is a medium melt flow rate heterophasic copolymer with suitable additives to produce caps and closures for carbonated beverages. This product exhibits high stiffness and impact strength bal..