Izod Impact, Notched 0.710 J/cm

@Temperature -30.0 °C
1.33 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp C7410 PC+ABS (Asia Pacific)
LNP* Thermocomp* C7410 compound is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 0.710 J/cm

@Temperature 23.0 °C
1.33 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Aspira EN177 Copolyester Resin for Extrusion Blow Molding
Applications:Beverage packagingConsumer packagingFood packagingPersonal care packagingKey Attributes:BPA-freeCompatible with high-output manufacturing platformsExcellent clarityHigh gloss appearance..