Mechanical Properties Metric English Comments
Izod Impact, Notched 0.625 J/cm

@Temperature -20.0 °C
1.17 ft-lb/in

@Temperature -4.00 °F
1/8" (3mm) notched bar; ASTM D256
Ineos L80Z-00 Impact Copolymer Polypropylene
L80Z-000 impact copolymer polypropylene is a high melt flow rate, nucleated and antistatic grade designed for high-speed injection molding applications. This resin meets the requirements of the U.S...