Polymer Property : Izod Impact, Notched = 0.418 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.418 J/cm

@Temperature -40.0 °C
0.783 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Provista NXT Copolymer Resin for Profile Extrusion
Applications:Candy packagingCorner guardsDisplays, Fixtures and Point of purchaseFood packagingFurniture guardsIntegrated circuit tubesLighting tubesPlastics for hygiene feminine productsPricing cha..