Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.177 J/cm @Temperature -20.0 °C |
0.331 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P401S Polypropylene Flat Yarn/Sheet Key Characteristics: Excellent mechanical propertiesRecommended Applications:Stretch tape for jumbo woven sheetMonofilament for rope and sheetInformation provided by SCG Chemicals |