Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.290 J/cm @Thickness 6.35 mm |
0.543 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
LG Chemical MI-730 MIPS |
|||
Izod Impact, Notched | 0.290 J/cm @Temperature -40.0 °C |
0.543 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar EN067 Copolyester, Natural Eastar Copolyester EN067 is a copolymer PET with good color. This product is supplied as a crystalline pellet that has improved flowability characteristics. Due to slower crystallization kinetics, t.. |